Martensitic alloys

 

Strengthen by heat treating

Fair corrosion resistance

410 is the basic martensitic alloy

  • 420: increase C (0.15, minimum) to increase strength
  • 440C: increase C (0.95-1.20) for high strength, hardness, and wear resistance
  • 416: add P and S to improve machinability compared to 410

 

SAE type C Mn Si Cr Ni
410 0.15 max 1.00 max 1.00 max 11.5 -13.0 -Fair general corrosion resistance
-High strength