Best combination of strength and corrosion resistance
Strengthen by heat treating
Contain small amounts of alloying elements that form microscopic particles within the alloy during heat treatment
Applications include: Components for aerospace, dental tools, automotive, and furnaces
SAE Type |
UNS |
C |
Mn |
Cr |
Ni |
Other |
13-8 Mo |
S13800 |
0.05, max |
0.2, max |
12.25 – 13.25 |
7.5 – 8.5 |
2.0-2.5 Mo, 0.9-1.35 Al, 0.01 N |
15-5 |
S15500 |
0.07, max |
1.00, max |
14.0 – 15.5 |
3.5 – 4.5 |
2.5-4.5 Cu, 0.15-0.45 Nb |
17-4 |
S17400 |
0.07, max |
1.00, max |
15.5 – 17.5 |
3.0 – 5.0 |
3.0-5.0 Cu, 0.15-0.45 Nb |